Skip to main content
Phosphinate based flame retardant for polyamides with improved GWIT performance

Exolit™ OP 1380

Exolit OP 1380 is a non-halogenated flame retardant based on organic phosphinates for reinforced polyamide 66 and polyamide 6. The product achieves its flame retardant effect through a combined gas phase and condensed phase mode of action. Compared to Exolit OP 1312, Exolit OP 1380 gives an improved performance in the glow wire ignition temperature (GWIT according to IEC 60695). Exolit OP 1380 is  based on a new chemical substance which is currently being registered in various national and regional chemical inventories.

For more details see our Innovation Spotlight video.

Benefits
  • Hich GWIT of at least 775°C in all thickness (0.75 mm - 3 mm)
  • UL 94 V-0 rating down to 0.4 mm thickness
  • The flame retardant polyamide compounds exhibit very good physical and excellent electrical properties
  • Low material density
  • Good colorability
  • Good contrast in laser marking
  • Non-halogenated flame retardants with favorable environmental and health profile
  • Shows a high potential for mechanical recycling while maintaining the flame retardancy and other properties

 

Safety

For regulatory details such as the classification and labelling as dangerous substances or goods please refer to our corresponding Material Safety Data Sheet. For disposal in accordance with the regulations the product should be treated as special waste and taken to a suitable incineration plant.

Technical Data

 

 

 

 Test method

Phosphorus

 % (w/w)

approx. 15.3

Photometry after oxidizing dissolution (11/17) or wavelength dispersive X-ray fluorescence spectrometry (11/23)

Moisture content

% (by wt.)

max. 1.0

 Karl-Fischer titration (11/21)

Density at 23°C

g/cm3

approx. 1.4

 

Bulk Density

kg/m3

approx. 490

 (DIN 53466)

Applications

Exolit OP 1380 was developed especially for use in polyamides. It is suited for polyamide 6 and 66 for both glass-fiber-reinforced and unreinforced grades. The flame retarded polyamide compounds exhibit very good physical and electrical properties.

Formulation

In glass-fiber-reinforced polyamide 6 or 6.6, a dosage of about 20 % (by wt.) of Exolit OP 1380 is usually sufficient to obtain GWIT of 775°C the UL 94 V-0 classification for electrical components (at 1.6 mm as well as 0.8 mm and 0.4 mm thickness). To achieve GWIT higher than 775°C we recommend increasing the dosage to about 23%. Subject to the polymer grade, processing conditions and glass-fiber-reinforcement the dosage of the flame retardant may vary.

Processing

Before incorporating Exolit OP 1380, it is important to pre-dry the polyamide as usual. If possible, the resulting moisture content should be below 0.1 % (by wt.). Pre-drying of Exolit OP 1380 is not necessary. However, pre-drying (e.g. 4 h at 120 °C) is recommended, if even very low moisture contents must be avoided.

The mixing and processing methods customary in powder processing of polymers can be used with Exolit OP 1380. The VDI Guideline 2263 Prevention of dust fires and dust explosions or the relevant national regulations must be observed.

The optimum conditions for incorporating should be determined in each individual case. Care must be taken to ensure homogeneous dispersion of all components. The temperature of the polymer melt should not exceed 320 °C.

Packaging and Handling

Delivery form
Powder

Packaging
Exolit OP 1380 is delivered in 20 kg bags.

Storage
The product should be stored in a dry place at room temperature. Opened containers should be tightly resealed after use.

Download File

Exolit™ OP 1380

Please choose one of the available product configurations:
No files are available for this product.

Login Required

Log in or register to ClariHub for our full set of ingredient documentation, formulations and more resources!

Page summary

Summarization in progress